钨铼合金
合金中添加Re元素,有效地改善了钨合金的塑性、降低了合金的韧脆转变温度,合金具有了更高的起始再结晶温度、抗蠕变性能和抗拉强度。
沈阳太普泰克钨钼科技有限公司为客户提供如下钨铼合金材料:
Description |
Symbol |
Chemical Composition |
Semifinished Products |
|||
processes |
sheet & plate Thickness /mm |
Rod Diameter /mm |
Wire Diameter /mm |
|||
TungstenRhenium Alloy |
W3Re |
3%(wt)Re, balance W |
Sintered/Forged/Drawn |
0.2-8 |
<18 |
0.025-1 |
W5Re |
5%(wt)Re, balance W |
Sintered/Forged/Drawn |
0.2-8 |
<18 |
0.5-1 |
|
W25Re |
25%(wt)Re, balance W |
Sintered/Forged/Drawn |
0.2-8 |
<18 |
0.5-1 |
|
W26Re |
26%(wt)Re, balance W |
Sintered/Forged/Drawn |
0.2-8 |
<18 |
0.5-1 |
|